<?xml version="1.0" encoding="UTF-8"?><rss version="2.0"
	xmlns:content="http://purl.org/rss/1.0/modules/content/"
	xmlns:wfw="http://wellformedweb.org/CommentAPI/"
	xmlns:dc="http://purl.org/dc/elements/1.1/"
	xmlns:atom="http://www.w3.org/2005/Atom"
	xmlns:sy="http://purl.org/rss/1.0/modules/syndication/"
	xmlns:slash="http://purl.org/rss/1.0/modules/slash/"
	>

<channel>
	<title>Uncategorized | פלסטיקה הנדסית</title>
	<atom:link href="https://www.sal-plastic.co.il/category/uncategorized/feed/" rel="self" type="application/rss+xml" />
	<link>https://www.sal-plastic.co.il</link>
	<description>לוחות ומוטות פלסטיק לצרכי עיבוד בתעשיות שונות: רפואי,מזון,כימיה,תעופתח, בטחוני ועוד &#124; מקבוצת ש.אל בע״מ</description>
	<lastBuildDate>Wed, 18 Oct 2023 13:08:15 +0000</lastBuildDate>
	<language>he-IL</language>
	<sy:updatePeriod>
	hourly	</sy:updatePeriod>
	<sy:updateFrequency>
	1	</sy:updateFrequency>
	<generator>https://wordpress.org/?v=5.8.8</generator>

<image>
	<url>https://www.sal-plastic.co.il/wp-content/uploads/2019/01/favicone-150x150.png</url>
	<title>Uncategorized | פלסטיקה הנדסית</title>
	<link>https://www.sal-plastic.co.il</link>
	<width>32</width>
	<height>32</height>
</image> 
	<item>
		<title>נקודות שחורות בחומרים פלסטיים חצי מוגמרים</title>
		<link>https://www.sal-plastic.co.il/%d7%a0%d7%a7%d7%95%d7%93%d7%95%d7%aa-%d7%a9%d7%97%d7%95%d7%a8%d7%95%d7%aa-%d7%91%d7%97%d7%95%d7%9e%d7%a8%d7%99%d7%9d-%d7%a4%d7%9c%d7%a1%d7%98%d7%99%d7%99%d7%9d-%d7%97%d7%a6%d7%99-%d7%9e%d7%95%d7%92/</link>
		
		<dc:creator><![CDATA[Amit Paz]]></dc:creator>
		<pubDate>Wed, 18 Oct 2023 13:03:28 +0000</pubDate>
				<category><![CDATA[Uncategorized]]></category>
		<guid isPermaLink="false">https://www.sal-plastic.co.il/?p=2675</guid>

					<description><![CDATA[<p>הופעתן של נקודות שחורות בחומר מעובד לעיתים במהלך העיבוד השבבי מתגלות נקודות שחורות בחומר הגלם. מדוע? הנקודות נוצרות בגלל פירוק שרשרת הפחמנים (C-C-C-C) של הפולימר לפחמן חופשי (C) בזמן חשיפה לחום וחמצן בשלב הפילמור מתי? כאשר ישנה החלפה בייצור, בין סוגים שונים של פולימרים, וכן כשיש הבדל בין טמפרטורות הייצור של החומרים כיצד? החומר &#34;השחור&#34; [&#8230;]</p>
<p>הפוסט <a rel="nofollow" href="https://www.sal-plastic.co.il/%d7%a0%d7%a7%d7%95%d7%93%d7%95%d7%aa-%d7%a9%d7%97%d7%95%d7%a8%d7%95%d7%aa-%d7%91%d7%97%d7%95%d7%9e%d7%a8%d7%99%d7%9d-%d7%a4%d7%9c%d7%a1%d7%98%d7%99%d7%99%d7%9d-%d7%97%d7%a6%d7%99-%d7%9e%d7%95%d7%92/">נקודות שחורות בחומרים פלסטיים חצי מוגמרים</a> הופיע לראשונה ב-<a rel="nofollow" href="https://www.sal-plastic.co.il">פלסטיקה הנדסית</a>.</p>
]]></description>
										<content:encoded><![CDATA[		<div data-elementor-type="wp-post" data-elementor-id="2675" class="elementor elementor-2675">
						<div class="elementor-inner">
				<div class="elementor-section-wrap">
									<section class="elementor-section elementor-top-section elementor-element elementor-element-6f31d51 elementor-section-boxed elementor-section-height-default elementor-section-height-default" data-id="6f31d51" data-element_type="section">
						<div class="elementor-container elementor-column-gap-default">
							<div class="elementor-row">
					<div class="elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-ebdc25c" data-id="ebdc25c" data-element_type="column">
			<div class="elementor-column-wrap elementor-element-populated">
							<div class="elementor-widget-wrap">
						<div class="elementor-element elementor-element-a130d77 elementor-widget elementor-widget-text-editor" data-id="a130d77" data-element_type="widget" data-widget_type="text-editor.default">
				<div class="elementor-widget-container">
								<div class="elementor-text-editor elementor-clearfix">
				<p><u><b>הופעתן של נקודות שחורות בחומר מעובד</b></u></p><p>לעיתים במהלך העיבוד השבבי מתגלות נקודות שחורות בחומר הגלם.</p><ul><li><b>מדוע? </b>הנקודות נוצרות בגלל פירוק שרשרת הפחמנים (C-C-C-C) של הפולימר לפחמן חופשי (C) בזמן חשיפה לחום וחמצן בשלב הפילמור</li><li><b>מתי? </b>כאשר ישנה החלפה בייצור, בין סוגים שונים של פולימרים, וכן כשיש הבדל בין טמפרטורות הייצור של החומרים</li><li><b>כיצד? </b>החומר &quot;השחור&quot; נדבק על דפנות בורג האקסטרודר או על חלקים שונים במכונה ומתערבב עם החומר התקין</li></ul><p>כיום לא קיימת תקינה לכמות, פיזור וקוטר של נקודות אלו &#8211; כל יצרן קובע את הסטנדרט שלו, אך הפרקטיקה המקובלת בתעשייה היא שחומר תקין ייחשב לכזה שיש לו 1-2 נקודות ל- square feet וקוטר נקודה מקסימלי של &quot;1/32.</p><p>לסיכום, נקודות שחורות בפולימר במוצרים חצי מוגמרים אינן משפיעות על איכות החומר ומהוות בעיקר בעיה אסתטית שנעשים מאמצים רבים כדי למנוע אותה, במסגרת הסטנדרטים המקובלים בתעשייה.</p><p> </p><p><strong><a href="https://www.sal-plastic.co.il/wp-content/uploads/2023/10/נקודות-שחורות-003.pptx-.pdf">לדף המצגת</a></strong></p>					</div>
						</div>
				</div>
						</div>
					</div>
		</div>
								</div>
					</div>
		</section>
									</div>
			</div>
					</div>
		<p>הפוסט <a rel="nofollow" href="https://www.sal-plastic.co.il/%d7%a0%d7%a7%d7%95%d7%93%d7%95%d7%aa-%d7%a9%d7%97%d7%95%d7%a8%d7%95%d7%aa-%d7%91%d7%97%d7%95%d7%9e%d7%a8%d7%99%d7%9d-%d7%a4%d7%9c%d7%a1%d7%98%d7%99%d7%99%d7%9d-%d7%97%d7%a6%d7%99-%d7%9e%d7%95%d7%92/">נקודות שחורות בחומרים פלסטיים חצי מוגמרים</a> הופיע לראשונה ב-<a rel="nofollow" href="https://www.sal-plastic.co.il">פלסטיקה הנדסית</a>.</p>
]]></content:encoded>
					
		
		
			</item>
	</channel>
</rss>